Poor printing methods at the beginning of printing
Analysis of the causes of this problem may be the following:
1. Not using the specified glue or glue solution too thick 2, uneven coating 3, drying temperature is too high 4, contact with strong light after coating 5, plated in a high temperature and humidity environment
It is recommended to take the following measures:
1. Use Fuji star light accessory products PP-I type PS plate protection glue (manual) or PP-IIxxxx type PS plate protection glue (machine)
2. Dilute the glue properly 3, Hand-glue to make it clean and dry 4. Set the drying temperature to below 60 degrees 5, Protect from light after gluing, 6. Do not store under high temperature and high humidity conditions.