First look: mainly to observe whether the surface gloss of the laminate flooring is uniform, whether the pattern is symmetrical, whether there are white spots or stains; whether the interface is neat and undamaged, whether there are tiny sawtooth cracks; whether there are detailed Chinese and English manuals at the same time; Regular verification report issued, whether the content of the report has been altered.
Second touch: Carefully touch the surface of the wooden floor with your hand, whether there is a feeling of unevenness.
Sanwen: Can you smell a noticeable pungent smell?
Four tests: Although consumers do not have equipment, they can still identify composite wood flooring through simple testing methods.
In order to test the abrasion resistance of the composite wood floor, it can be sanded back and forth 10 to 20 times with the No. 108 sandpaper. If the pattern breaks, it belongs to the unqualified floor without wear layer; if it is polished 20 to 40 times, the pattern appears obviously damaged. It is a poor wear-resistant floor.
The surface resistance to cigarette burning is determined by the ability of the wear-resistant layer on the surface of the reinforced composite wood flooring product to ignite the burning of the cigarette, which reflects the flame retardant performance of the surface of the product to some extent. Ignite the cigarette and suck it about 10 mm, place it on the surface of the laminate flooring for 1 minute, remove the cigarette, then suck about 10 mm, place it on the surface of the product at another point, and remove the cigarette after 1 minute. Cigarettes cannot self-extinguish throughout the process, otherwise they are re-tested. It is then observed that if there is no significant change in the surface of the wooden floor, it is a qualified product.
In the trial paving, the gap in the middle of the wooden floor can be carefully observed. The standard of the qualified composite wooden floor is not more than 0.2 mm, and the average value is not more than 0.15 mm. The height difference of the wooden floor is 0.15 mm and the average value is 0.1 mm.
In order to test the stain resistance of the composite wood floor, the soy sauce, vinegar and cooking oil can be poured on the surface of the floor a little, and then scrubbed. If no trace is left, it is a qualified product.